About Accumet Materials Co.

 

Accumet Materials Co.

 
     

 

   

 

 

 

 

 

 

REFRACTOCOAT ALS, SIS AND MGS
 HIGH TEMPERATURE CERAMIC COATINGS

 

APPLICATION PROCEDURES

 

Surface Preparation

Clean surfaces thoroughly prior to application.  Extremely smooth surfaces should be roughened by sanding or sandblasting.  Porous substrates should be brushed with clean water or pre-coated with a thin layer of coating to avoid wicking.

 

Mixing

REFRACTOCOAT Coatings should be thoroughly mixed to a uniform consistency.  Mix slowly to avoid air entrapment.  REFRACTOCOAT MGS two component system should be mixed 1.5 parts powder to 1.0 parts liquid by weight.

 

Application

Apply coatings thinly using a brush, spatula or dipping.  If spraying, the viscosity can be lowered by adding small amounts of water.  After coating is applied, air dry for 4 hours until it has hardened.  If several applications are required, allow the coating to air dry before applying second coat.  A 200 ºF heat cure is also recommended for each successive coat to avoid bubbling and blistering.

 

Curing

All coatings should air dry for 4 hours, then heat cured at 175 ºF for 4 hours to remove residual moisture.  For best results, proceed with step firing at 200 ºF for 1 hour, 500 ºF for 1 hour and 700 ºF for 1 hour.

 

Safety

Accumet’s REFRACTOCOAT high temperature ceramic coatings can be cleaned from brushes, spatulas and spraying equipment with soap and water.  Wash from skin with soap and warm water.  Prolonged skin contact should be avoided to prevent skin irritation.  See MSDS for additional handling.

 

Storage

REFRACTOCOAT ALS, SIS, MGS should be stored at room temperature and high humidity environments should be avoided.  Typical shelf life is 6-12 months. 

 

Accumet Materials Co. accepts Visa & Mastercard

 Call us at (914)762-1540, Fax us at (914) 762-1291 or
  E-Mail us at
sales@accumetmaterials.com

Having a problem with this site?. mail to: WebMaster

Home | FAQ | Links | Site Index | About